Review Paper on Partial Replacement of Fine Aggregate
2018-4-20 · (normal concrete mix), three mix including lime stone waste 25%, 50% and 75% replacement from sand. Twelve mixes including lime stone waste with marble powder as additive by percent 5, 10, and 15% by weight of cement. Phase-II, the above experiment is repeated with cement content is 450 kg/ m3. Compression test at7, 28, and 90